Heres a job I just sent back to its owner in Connecticut.

ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4003.jpg


ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4002.jpg


ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4006.jpg


ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4004.jpg


ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4008.jpg


ai25.photobucket.com_albums_c74_olyeller14_kahrs_DSCN4009.jpg
 

grwd

Sharpshooter
Joined
Jan 22, 2006
Messages
11,245
Reaction score
118
Location
usa
honestly, a bare s.s. finish is a b!tch to melt. I go through about 6 grits of sanding to get it good enough to bead blast and call it good.
 