are you still selling the linotype?
I still have a dozen or so of the 40# slugs left that end up being 2/3 Linotype when smelted to ingots. I am sending samples of the smelted slugs off to have analyzed to confirm tin and antimony is the same as the first samples I sent off. I do have both 95% tin solder and Lino that is for sale
 
Joined
May 20, 2017
Messages
310
Reaction score
184
Location
Tulsa
For really slow 30 cal I found the short Lee .311-100-2R bullet groups better than the longer 170 gr. or 230 gr. bullet. That .311 is made for the 32-20 etc etc.
Turns out I have the lyman 311316 and 311356 molds, have not used and not sure what the as cast diameter will be. 120 grain but both gas check. I may give those a try as 1,000 or less fps 30/30 and 300BO single load rounds for the kids.
 
Joined
May 20, 2017
Messages
310
Reaction score
184
Location
Tulsa
While the posted pictures may look the same, they are different. Smelted over 600# of the used Linotype into ingots starting at 9 this morning and finishing at 3 in the afternoon. had to carry the 600# of raw material about 50 yards around the corner of the barn, 30# to 50# slugs, one at a time. home now and ready for an adult Bev and getting my feet up.
Lead recycler has sent me 9 steel 5 gallon buckets. Will load each up with about 90# of the fines from the lead and strap to a heavy duty pallet next week. they are paying shipping to return to their factory. analysis showed 10% tin, 20% antimony, remanded lead. depending of shipping cost, maybe I will have some positive credit to buy pure lead.
A couple of weeks ago I did buy a second cast iron 3x3 ingot mold. each ingot about 2.5#. really helped speed up with the pouring of ingot.
Picture is 290# of lead. another rack has around 27 of the 6.25# triangle ingots from the angle iron molds I made. probably 1/3 of the time was fluxing and getting the fines out of the pot. My first 450# smelt day. 7 slugs, around 250#, and 150# of COWW are all the raw material I have left. Then I will be thru smelting, at least for now.
 

Attachments

  • lead lino 300#.JPG
    lead lino 300#.JPG